Hardener Additive TPUA - ACFN (NON YELLOWISH) |
|
DESCRIPITON
|
|||||||||||||||
|
The almost colorless TPUA-ACFN (NON YELLOWISH) is designed as curing agent for adhesive based on hydroxyl polyurethane, natural and synthetic rubber; owing to TPUA-ACFN (NON YELLOWISH) features good photo-resistance, it is particularly suitable for light-color polyurethane adhesive system. Because the solvent is ethyl acetate, TPUA-ACFN (NON YELLOWISH) can be used in those countries where the use of methylene chloride is restricted.
|
|||||||||||||||
| TYPICAL PROPERTIES | |||||||||||||||
|
|||||||||||||||
| PERFORMANCE | |||||||||||||||
| The
Film of adhesive and coasting film mixed by TPUA-ACFN (NON YELLOWISH), is
difficult to become yellow after exposure to UV light and heat. So TPUA-ACFN
(NON YELLOWISH) shows good bonding strength in PVC with much plasticizer,
SBR with plenty of oil, coasting leather, silk and so on. |
|||||||||||||||
| APPLICATION | |||||||||||||||
|
After the addition of TPUA-ACFN (NON YELLOWISH), the ready-to-use double-component adhesive should be applied within a period (pot life) which is determined not only its content of rubber, but also by the other ingredients of the formulation (e.g. resins, antioxidants, solvents, etc.) If the adhesive is not used within this period, it may become increasingly difficult to apply and its viscosity increases rapidly until irreversible gelling ultimately occurs.
|
|||||||||||||||
| SUGGESTED ADDITIONS | |||||||||||||||
For
Curing adhesive of 100 parts by weight (p.b.w) based on:
|
|||||||||||||||
| PACKAGE | |||||||||||||||
| A.
each 0.8kg in a standard aluminum bottle B. each 20 bottles in a standard carton C. each 180kg in an iron drum |
| Notice: These values are based on the test of our present laboratory test specimens. |